Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
Manufacturer Techmer ES
Trade Name Electrablend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Water Absorption 0.14 %

@Time 86400 sec
0.14 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0015 cm/cm

@Thickness 3.17 mm
0.0015 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Yield 110 MPa
16000 psi
ASTM D638
Elongation at Break 1.8 %
1.8 %
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 11.9 GPa
1730 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 2.67 J/cm

@Thickness 3.17 mm
5.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 10 - 1000 ohm-cm
10 - 1000 ohm-cm
ASTM D257
Surface Resistance 10 - 10000 ohm
10 - 10000 ohm
ASTM D257