Techmer ES Elastoblend® PBT GF33 IM 33% Glass Filled

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Techmer ES
Trade Name Elastoblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Elastoblend® PBT GF33 IM 33% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Water Absorption 0.050 %

@Time 86400 sec
0.050 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 117 MPa
17000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Yield Strength 172 MPa
25000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm

@Thickness 6.35 mm
2.40 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 25.2 µm/m-°C
14.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 224 °C
435 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
402 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in