Taiwan PU Corporation TPU-E98 General Grade, Extrusion Molding Polyester Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPU-E98 General Grade, Extrusion Molding Polyester Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 98
98
Tensile Strength at Break 41.19 MPa
5974 psi
Elongation at Break 650 %
650 %
100% Modulus 0.0118 GPa
1.71 ksi
300% Modulus 0.0245 GPa
3.55 ksi
Resilience 26
26
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 5.0
5.0
Processing Properties Metric English Comments
Feed Temperature 195 °C
383 °F
Middle Barrel Temperature 200 °C
392 °F
Compress zone
Front Barrel Temperature 205 °C
401 °F
Metering zone
Adapter Temperature 215 °C
419 °F
Die Temperature 215 °C
419 °F