TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 300ºF Cure Temperature

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 300ºF Cure Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.FormulationMillathane HT100.0Zinc Stearate0.5MBTS4.0MBT2.0N-330 Black20.0Sulfur1.5THANECURE® ZM1.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
Tensile Strength, Yield 27.16 MPa
3939 psi
Elongation at Yield 403 %
403 %
100% Modulus 0.00312 GPa
0.452 ksi
200% Modulus 0.008467 GPa
1.228 ksi
300% Modulus 0.01576 GPa
2.286 ksi
Tear Strength 51.8 kN/m
296 pli
Die C
Processing Properties Metric English Comments
Cure Time 25.0 min

@Temperature 149 °C
0.417 hour

@Temperature 300 °F