Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 6.0 PHR MBTS

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 6.0 PHR MBTS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100Zinc Stearate0.5N330 Black30.0Cumar P1010.0MBT2.0Thanecure® ZM1.0Sulfur1.5MBTS6.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 66
>= 66
Tensile Strength, Yield 27.39 MPa
3973 psi
Elongation at Yield 485 %
485 %
100% Modulus 0.00320 GPa
0.464 ksi
200% Modulus 0.006998 GPa
1.015 ksi
300% Modulus 0.01210 GPa
1.755 ksi
Tear Strength 32.6 kN/m
186 pli
Die C
Compression Set 36.6 %

@Temperature 70.0 °C,
Time 79200 sec
36.6 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 12.5 min

@Temperature 155 °C
0.208 hour

@Temperature 311 °F