TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Hi-Sil 233 Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 60 PHR Hi-Sil 233 Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0Zinc Stearate0.5MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5Cumar P1010.0Precipitated Silica - Hi-Sil 23360All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 78
>= 78
Tensile Strength, Yield 25.1 MPa
3640 psi
Elongation at Yield 760 %
760 %
100% Modulus 0.00200 GPa
0.290 ksi
200% Modulus 0.00320 GPa
0.464 ksi
300% Modulus 0.00480 GPa
0.696 ksi
Tear Strength 32.5 kN/m
185 pli
Die C
Processing Properties Metric English Comments
Cure Time 16.0 min

@Temperature 68.3 °C
0.267 hour

@Temperature 155 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 65.3