Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N550 (FEF) Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N550 (FEF) Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0Zinc Stearate0.5Struktol WB 2220.5Poly AC 617A0.5Cumar P1010.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5Carbon Black N-550 (FEF)20All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 60
>= 60
Tensile Strength, Yield 29.19 MPa
4234 psi
Elongation at Yield 594 %
594 %
100% Modulus 0.00190 GPa
0.276 ksi
200% Modulus 0.00410 GPa
0.595 ksi
300% Modulus 0.007198 GPa
1.044 ksi
Tear Strength 39.8 kN/m
227 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 68.3 °C
0.167 hour

@Temperature 155 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 51.7
Copyright © lookpolymers.com All Rights Reserved