Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.5 PHR Sulfur.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100Zinc Stearate0.5N330 Black30.0Cumar P1010.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur0.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 58
>= 58
Tensile Strength, Yield 24.19 MPa
3509 psi
Elongation at Yield 684 %
684 %
100% Modulus 0.00170 GPa
0.247 ksi
200% Modulus 0.00340 GPa
0.493 ksi
300% Modulus 0.00590 GPa
0.856 ksi
Tear Strength 34.3 kN/m
196 pli
Die C
Compression Set 39.5 %

@Temperature 70.0 °C,
Time 79200 sec
39.5 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 155 °C
0.250 hour

@Temperature 311 °F