TSE Industries Millathane® CM Millable Polyether Urethane Rubber with DOP Plasticizer

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber with DOP Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N-330 Carbon Black30.0DOP15.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.50All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
63
63
aged in air at 100ºC for 4 days
Tensile Strength, Yield 22.8 MPa
3300 psi
aged in air at 100ºC for 4 days
26.2 MPa
3800 psi
Elongation at Break 350 %
350 %
aged in air at 100ºC for 4 days
470 %
470 %
300% Modulus 0.0131 GPa
1.90 ksi
0.01810 GPa
2.625 ksi
aged in air at 100ºC for 4 days