Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 287ºF Cure Temperature

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® CM Millable Polyether Urethane Rubber, 287ºF Cure Temperature.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subjected to high wear in service. It has a unique combination of excellent properties, such as low temperature characteristics, and resistance to heat deterioration, ozone cracking, weathering and swelling in oils or solvents.FormulationMillathane CM 100.0N330 Carbon Black30.0Coumarone-Indene Resin15.0MBTS4.0MBT1.0Sulfur0.75CAYTUR 40.35Zinc Stearate0.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 65
65
Tensile Strength, Yield 34.8 MPa
5050 psi
Elongation at Break 570 %
570 %
300% Modulus 0.01086 GPa
1.575 ksi
Compression Set 23 %

@Temperature 70.0 °C,
Time 79200 sec
23 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 142 °C
1.00 hour

@Temperature 287 °F
Descriptive Properties Value Comments
500% Modulus (ksi) 3.55
Users viewing this material also viewed the following: