Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications.All information provided by TSE Industries
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
Mooney Viscosity 25 - 45

@Temperature 100 °C
25 - 45

@Temperature 212 °F
Standard; ML(1+4)
25 - 70

@Temperature 100 °C
25 - 70

@Temperature 212 °F
ML(1+4)
Mechanical Properties Metric English Comments
Hardness, Shore A 30 - 90
30 - 90
Tensile Strength, Yield 31.0 MPa
4500 psi
Elongation at Yield 500 %
500 %
Resilience 10 - 20
10 - 20
%
Thermal Properties Metric English Comments
Brittleness Temperature -40.0 °C
-40.0 °F
Descriptive Properties Value Comments
Appearance Light to dark amber solid bale or milled sheets
Compression Set Very Good
Peroxide Cure
Health Hazard None
Heat Aging Resistance Good at 100ºC
sulfur cure
Very Good at 100ºC
peroxide cure
Ozone Resistance Excellent
Storage Stability Excellent
Tear Resistance Very Good
Sulfur Cure
Weather Resistance Good