Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 80A, Black Peroxide Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Stearic Acid0.5TP-9510.0N-77470.0SR 2977.5Di-Cup 40C3.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 80
80
Tensile Strength, Yield 18.22 MPa
2642 psi
Elongation at Yield 251 %
251 %
100% Modulus 0.00680 GPa
0.986 ksi
200% Modulus 0.01620 GPa
2.349 ksi
Tear Strength 35.0 kN/m
200 pli
Die C
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 160 °C
0.250 hour

@Temperature 320 °F
Copyright © lookpolymers.com All Rights Reserved