Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Sulfur Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Black Sulfur Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5N-550 Black15.0TP-955.0MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 28.76 MPa
4171 psi
Elongation at Yield 564 %
564 %
100% Modulus 0.00227 GPa
0.329 ksi
200% Modulus 0.00498 GPa
0.723 ksi
300% Modulus 0.008770 GPa
1.272 ksi
Tear Strength 59.9 kN/m
342 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 155 °C
0.167 hour

@Temperature 311 °F
Copyright © lookpolymers.com All Rights Reserved