TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Non-Black Sulfur Cure

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 50A, Non-Black Sulfur Cure.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems.FormulationMillathane 76 100.0Zinc Stearate0.5AC Poly 617A2.0Hi-Sil 23310.0Titanium Dioxide5.0MBTS4.0MBT1.0Thanecure® ZM1.0Sulfur1.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 50
50
Tensile Strength, Yield 34.43 MPa
4993 psi
Elongation at Yield 643 %
643 %
100% Modulus 0.00155 GPa
0.225 ksi
200% Modulus 0.00263 GPa
0.381 ksi
300% Modulus 0.00456 GPa
0.662 ksi
Tear Strength 47.1 kN/m
269 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 155 °C
0.167 hour

@Temperature 311 °F