Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Sulfur

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Sulfur.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Like many oil resistant synthetic rubbers, Millathane 76 requires a treated grade of sulfur to ensure proper dispersion.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength, Yield 33.16 MPa
4809 psi
Elongation at Yield 588 %
588 %
100% Modulus 0.00331 GPa
0.480 ksi
200% Modulus 0.007460 GPa
1.082 ksi
300% Modulus 0.01316 GPa
1.909 ksi
Tear Strength 59.7 kN/m
341 pli
Die C
Compression Set 27.1 %

@Temperature 70.0 °C,
Time 79200 sec
27.1 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 8.80 min

@Temperature 155 °C
0.147 hour

@Temperature 311 °F
TC90