TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 0.0 PHR Thanecure ZM.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and many other high performance polyurethane applications. Millathane 76 can be vulcanized by sulfur or peroxide cured systems. Thanecure ZM is an activator for a sulfur cure of Millathane® millable polyurethanes consisting of a partial complex of zinc chloride and MBTS.All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
Tensile Strength, Yield 27.56 MPa
3997 psi
Elongation at Yield 628 %
628 %
100% Modulus 0.00245 GPa
0.356 ksi
200% Modulus 0.00534 GPa
0.774 ksi
300% Modulus 0.009487 GPa
1.376 ksi
Tear Strength 65.0 kN/m
371 pli
Die C
Compression Set 49.4 %

@Temperature 70.0 °C,
Time 79200 sec
49.4 %

@Temperature 158 °F,
Time 22.0 hour
Processing Properties Metric English Comments
Cure Time 34.2 min

@Temperature 155 °C
0.570 hour

@Temperature 311 °F
TC90