TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® KS150-600SP Primary Synthetic Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Applications: Copper friction parts copper clutch facingsInformation provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.670 g/cc
0.0242 lb/in³
Scott
0.770 g/cc
0.0278 lb/in³
Tap
Particle Size >= 250 µm
>= 250 µm
d50, 83%, Vibrated sieving
>= 500 µm
>= 500 µm
d90, 22%, Vibrated sieving
550 µm
550 µm
at a density of 2.16 g/cc
1000 µm
1000 µm
at a density of 2.12 g/cc
Deformation 1.4 %
1.4 %
plastic
1.4 %
1.4 %
elastic
2.8 %
2.8 %
plastic + elastic
Ash 0.060 %
0.060 %
Typical
Mechanical Properties Metric English Comments
Coefficient of Friction 0.59

@Temperature 850 °C,
Time 10800 sec
0.59

@Temperature 1560 °F,
Time 3.00 hour
Friction coefficient of sintered Cu-C -brake pads with 10% TIMREX® KS Graphite as a function of the particle size, Sinterdensity: 55% of the theoret. density
Abrasion 0.25

@Temperature 850 °C,
Time 10800 sec
0.25

@Temperature 1560 °F,
Time 3.00 hour
Friction coefficient and wear of sintered Cu-C -brake pads with 10% T 150-600 Graphite, Sinterdensity: 55% of the theoret. density
Thermal Properties Metric English Comments
Thermal Conductivity 140 W/m-K
972 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Moisture Content 0.040 %
0.040 %
Typical
Descriptive Properties Value Comments
Crystallite height Lc >100 nm
DBP absorption 17 g/100g
(Dibutylphthalate)