Synergy Polymers Ultra Purge Plus

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Synergy Polymers
Trade Name Ultra Purge
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Synergy Polymers Ultra Purge Plus.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents. Moldable compound. For use with: Injection Molding Machines Hot Runners Extruders Blow Molding Machines without accumulators Purged Resin: All purpose usageInformation provided by Synergy Polymers.
Physical Properties Metric English Comments
Density 0.700 g/cc
0.0253 lb/in³
Thermal Properties Metric English Comments
Melting Point 70.0 °C
158 °F
Maximum Service Temperature, Air 320 °C
608 °F
Minimum Service Temperature, Air 190 °C
374 °F
Decomposition Temperature >= 85.0 °C
>= 185 °F
Avoid temperature > 80°C except during use
Flammability Test >= 300
>= 300
[°C] In flammability point
>= 450
>= 450
[°C] Ignition temperature