Sylvin Technologies 9950-90 Natural PVC Molding Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9950-90 Natural PVC Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
10 seconds
Tensile Strength, Ultimate 12.8 MPa
1850 psi
Elongation at Break 260 %
260 %
Tear Strength Test 390
390
Processing Properties Metric English Comments
Melt Temperature 171 - 182 °C
340 - 360 °F