Sylvin Technologies 9812A-70 Natural PVC for Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Sylvin Technologies
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sylvin Technologies 9812A-70 Natural PVC for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
Thickness 1000 microns
39.4 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
10 seconds
Tensile Strength, Ultimate 10.0 MPa
1450 psi
Elongation at Break 375 %
375 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
RTI
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 160 - 171 °C
320 - 340 °F