Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Suzhou Hipro Polymers Hipromin® 102 1.10 Decamethylenediamine

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Suzhou Hipro Polymers
Trade Name Hipromin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suzhou Hipro Polymers Hipromin® 102 1.10 Decamethylenediamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hipromin® 102 (1.10-Decamethylenediamine) is widely used for long chain polyamide polymerization, molecular weight regulation, cross linking, etc.Information provided by Suzhou Hipro Polymers Co. Ltd
Physical Properties Metric English Comments
Solubility 1.00e+6 ppm
1.00e+6 ppm
in ethanol
Thermal Properties Metric English Comments
Melting Point >= 60.0 °C
>= 140 °F
GB4608
Descriptive Properties Value Comments
Color < 25
APHA 20% ethanol
Purity > 98%
Test Method: GC