Material Notes:
Chemical Name: 4-Hydroxy-2,2,6,6-tetramethyl-piperidinooxy (TMHPO')CAS NO.: 2226-96-2Molecular Formula: C9H18NO2Uses: It can prevent alkene from self-polymerization, or control and adjust the degree of polymerization.Information Provided by Suqian Unitechem Co., Ltd.
Physical Properties Metric English Comments
Molecular Weight 172.25 g/mol
172.25 g/mol
Ash 0.10 %
0.10 %
Thermal Properties Metric English Comments
Melting Point 69.0 - 72.0 °C
156 - 162 °F
Descriptive Properties Value Comments
Appearance Orange red crystal
Assay (%) 99
GC
Weight Loss (%) 0.5