Material Notes:
Characteristics Medium flow High Impact Excellent formability Low temperature toughnessProcessing Extrusion Molding FormingApplications Thermoformed containers, extruded profiles, packaging products Plates, dishes, disposable cups, deep drawn thermoformed containers Also suitable for audio/video cabinets, business machines, ball pen etc.Material Status: Commercial : ActiveAgency Ratings: FDA 21 CFR 177.1640, UL file E185934Information provided by Supreme Petrochem LTD
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.4 MPa
4120 psi
50 mm/min; ASTM D638
Elongation at Break 50 %
50 %
50 mm/min; ASTM D638
Flexural Strength 43.1 MPa

@Thickness 3.20 mm
6250 psi

@Thickness 0.126 in
ASTM D790
Flexural Modulus 1.86 GPa

@Thickness 3.20 mm
270 ksi

@Thickness 0.126 in
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 3.20 mm
2.06 ft-lb/in

@Thickness 0.126 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
ASTM D648
Vicat Softening Point 102 °C
216 °F
1kg / 120°C; ASTM D1525
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Processing Properties Metric English Comments
Melt Temperature 180 - 260 °C
356 - 500 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F