Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Injection Grade

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Glass Filled
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Sumikon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite Sumikon® PM-9610 Glass-Filled Phenolic, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sumikon PM-9610 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and higher dimensional stability with excellent heat resistance. Typical applications include brush holders for high temperature, and timing pulleys.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.02 g/cc
2.02 g/cc
ASTM D792
Bulk Density 0.960 g/cc
0.0347 lb/in³
ASTM D1895
Bulk Factor 2.1
2.1
ASTM D1895
Water Absorption 0.030 %
0.030 %
ASTM D570
Linear Mold Shrinkage 0.0025 cm/cm
0.0025 in/in
ASTM D6289
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 96.0 MPa
13900 psi
ASTM D638
Tensile Modulus 24.8 GPa
3600 ksi
ASTM D638
Flexural Strength 172 MPa
24900 psi
ASTM D790
Compressive Strength 241 MPa
35000 psi
ASTM D695
Izod Impact, Notched 0.214 J/cm
0.401 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 4.9

@Frequency 1e+6 Hz
4.9

@Frequency 1e+6 Hz
ASTM D150
5.0

@Frequency 1000 Hz
5.0

@Frequency 1000 Hz
ASTM D150
5.1

@Frequency 60 Hz
5.1

@Frequency 60 Hz
ASTM D150
Dielectric Strength 9.84 kV/mm
250 kV/in
Step by Step; ASTM D149
15.0 kV/mm
380 kV/in
Short Time; ASTM D149
Dissipation Factor 0.030

@Frequency 1000 Hz
0.030

@Frequency 1000 Hz
ASTM D150
0.030

@Frequency 1e+6 Hz
0.030

@Frequency 1e+6 Hz
ASTM D150
0.040

@Frequency 60 Hz
0.040

@Frequency 60 Hz
ASTM D150