Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America SI 9045C Silicone Compound

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America SI 9045C Silicone Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Long fiberglass and graphite filled silicone molding compound which offers moderate strength properties, high impact resistance, and excellent thermal stability at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
Relative Density; ASTM D792
Water Absorption 0.45 %
0.45 %
48 hr @ 50°C; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
Compression Molding; ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
ASTM D2583
Tensile Strength at Break 17.0 MPa
2470 psi
ASTM D638
Flexural Strength 52.0 MPa
7540 psi
At Rupture; ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
ASTM D790
Compressive Strength 55.0 MPa
7980 psi
ASTM D695
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 282 °C
>= 540 °F
Post Baked; ASTM D648A
Descriptive Properties Value Comments
Color Black
Form Coarse Flake - 1/4" Chop
Main Filler Glass Fiber & Graphite
Molding Method Compression, transfer
Users viewing this material also viewed the following: