Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Fabric Filled
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Military Specification MIL-M-14H.)Information supplied by Sumitomo Bak North America.
Physical Properties Metric English Comments
Bulk Density 0.300 g/cc
0.0108 lb/in³
Powder; ASTM D1895
Density 1.38 g/cc
0.0499 lb/in³
ASTM D-792
Water Absorption 0.60 %
0.60 %
24 hour; ASTM D570
2.2 %
2.2 %
48 hour; ASTM D570
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 105
105
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Flexural Strength 86.0 MPa
12500 psi
ASTM D790
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Compressive Strength 165 MPa
23900 psi
ASTM D695
Izod Impact, Notched 1.03 J/cm
1.93 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Maximum Service Temperature, Air 150 °C
302 °F
UL Temperature Index; UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
As Molded; ASTM D648A
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Dielectric Strength 3.10 kV/mm
78.7 kV/in
60 Hz, wet, SS; ASTM D149
5.50 kV/mm
140 kV/in
ST; ASTM D149
Descriptive Properties Value Comments
Available Molding Grades Compression, Transfer, Injection
Color Black
Form Pellet
Copyright © lookpolymers.com All Rights Reserved