Sumitomo Bakelite North America E 7459A Long Glass Fiber Reinforced Epoxy

Category Polymer , Thermoset , Epoxy , Epoxy, Molded, Glass Fiber Filler , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America E 7459A Long Glass Fiber Reinforced Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EM 7459A is a medium strength fiberglass reinforced epoxy molding compound, which features enhanced impact strength and toughness.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 115 MPa
16700 psi
ASTM D638
Flexural Strength 145 MPa
21000 psi
at rupture; ASTM D790
Izod Impact, Notched 2.92 J/cm
5.47 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color Green
Form Coarse Flake
Molding Method Compression
Transfer