Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade

Category Polymer , Thermoset , Phenolic , Phenolic; Unreinforced; Molded
Manufacturer Sumitomo Bakelite High Peformance Plastics
Trade Name Durez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite Durez® 32962 Phenolic Molding Compound, Compression Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Durez 32962 Black Phenolic is a medium impact, molding compound. It is designed for applications where additional mechanical strength is required. Typical applications include appliance housings where strength and appearance are important.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Water Absorption 0.50 %
0.50 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D6289
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 48.0 MPa
6960 psi
ASTM D638
Tensile Modulus 6.90 GPa
1000 ksi
ASTM D638
Flexural Strength 76.0 MPa
11000 psi
ASTM D790
Compressive Strength 207 MPa
30000 psi
ASTM D695
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C

@Thickness 3.00 mm
302 °F

@Thickness 0.118 in
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
360 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
V-0

@Thickness 6.00 mm
V-0

@Thickness 0.236 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D257
Dielectric Constant 6.0

@Frequency 1.00e+6 Hz
6.0

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 9.84 kV/mm
250 kV/in
Step by Step; ASTM D149
11.8 kV/mm
300 kV/in
Short Time; ASTM D149
Dissipation Factor 0.060

@Frequency 1.00e+6 Hz
0.060

@Frequency 1.00e+6 Hz
ASTM D150