Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styron XZ 92009.00 SB Latex

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XZ 92009.00 SB Latex.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: For use in oil well cements, gas blocking, high temperature gas migration controlApplications: Modified ConcreteEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 45.5 %
45.5 %
pH 11
11
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 12.0 °C
53.6 °F
Users viewing this material also viewed the following: