Styron XU 36535.00 Formulated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron XU 36535.00 Formulated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: ENVERSAâ„¢ Cushion Technology, excellent recovery, cushion, excellent acoustic propertiesApplications: Sound DampeningNorth AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 56 %
56 %
pH 8.0
8.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -50.0 °C
-58.0 °F