Styron Pulse® 930 ABS + Polycarbonate

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Styron
Trade Name Pulse®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Pulse® 930 ABS + Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PULSE® 930 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at room temperature. PULSE 930 Engineering resin has been used in automotive instrument panel and interior trim applications.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM Data
Melt Density 0.998 g/cc
0.0361 lb/in³
Melt density
Water Absorption 0.15 %
0.15 %
Moisture Absorption at Equilibrium 0.32 %
0.32 %
Humidity Absorption
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Melt Flow 3.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
3.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
Tensile Strength, Ultimate 55.2 MPa
8010 psi
ASTM Data
Tensile Strength, Yield 58.6 MPa
8500 psi
ASTM Data
Elongation at Break 100 %
100 %
ASTM Data
Elongation at Yield 4.2 %
4.2 %
ISO Data
Tensile Modulus 2.40 GPa
348 ksi
ISO Data.
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM Data
2.67 J/cm

@Temperature -50.0 °C
5.00 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data, Low Temp
NB
NB
ISO Data
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
ISO Data, Low Temp
5.60 J/cm²
26.7 ft-lb/in²
ISO Data
Impact Test 56.5 J

@Temperature -30.0 °C
41.7 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
56.5 J

@Temperature 23.0 °C
41.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Specific Heat Capacity 1.85 J/g-°C
0.442 BTU/lb-°F
Thermal Conductivity 0.227 W/m-K
1.58 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ASTM Data
121 °C
250 °F
annealed; ASTM Data