Styron Pulse® 600 ABS + Polycarbonate

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Styron
Trade Name Pulse®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron Pulse® 600 ABS + Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat resistance, and high impact strength at both room and low temperatures.Data provided by Dow Chemical.This product line was spun off from Dow Chemical to Styron in 2010.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM Data
Water Absorption 0.15 %
0.15 %
Moisture Absorption at Equilibrium 0.32 %
0.32 %
Humidity Absorption
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM Data
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
Tensile Strength, Ultimate 44.8 MPa
6500 psi
ASTM Data
Tensile Strength, Yield 51.0 MPa
7400 psi
ASTM Data
Elongation at Break 100 %
100 %
ASTM Data
Elongation at Yield 4.1 %
4.1 %
ISO Data
Tensile Modulus 2.30 GPa
334 ksi
ISO Data.
Izod Impact, Notched 3.74 J/cm
7.01 ft-lb/in
ASTM Data
2.14 J/cm

@Temperature -50.0 °C
4.01 ft-lb/in

@Temperature -58.0 °F
ASTM Data
Charpy Impact Unnotched NB
NB
ISO Data
NB
NB
ISO Data, Low Temp
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO Data, Low Temp
6.50 J/cm²
30.9 ft-lb/in²
ISO Data
Impact Test 56.5 J

@Temperature 23.0 °C
41.7 ft-lb

@Temperature 73.4 °F
Instrumented Dart Total Energy
62.2 J

@Temperature -30.0 °C
45.9 ft-lb

@Temperature -22.0 °F
Instrumented Dart Total Energy
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.8 µm/m-°C

@Temperature 20.0 °C
41.0 µin/in-°F

@Temperature 68.0 °F
ASTM data
Deflection Temperature at 1.8 MPa (264 psi) 98.9 °C
210 °F
Unannealed; 113°C (235°F) annealed; ASTM Data