Material Notes:
Performance Features: Excellent binding strength and durabilityApplications: Dust Control, Running Track and Soil StabilizationLatin America/South AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 50 %
50 %
pH 8.5
8.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 4.00 °C
39.2 °F