Styron LGF 7600 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron LGF 7600 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: STYRON LGF7600 is intended for use injection molding applications that require high stiffness. The material has good processability and fast cycle times. It contains nucleating agent. LGF 7600 can be used in combination with LGF glass concentrates for automotive applications.Applications:AutomotiveStructuralCombination with LGF glass concentratesInformation provided by Styron
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa

@Thickness 3.20 mm
4930 psi

@Thickness 0.126 in
Injection Molded; ASTM D638
Elongation at Yield 7.0 %

@Thickness 3.20 mm
7.0 %

@Thickness 0.126 in
Injection Molded; ASTM D638
Flexural Modulus 1.42 GPa
206 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.506 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
Injection Molded; ASTM D256