Styron DL 399 Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 399 Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Medium hard tough filmApplications: Thermo MoldableEuropeInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 54 %
54 %
pH 7.0
7.0
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 24.0 °C
75.2 °F