Material Notes:
Performance Features: Excellent binding strength and durability, robust compounding, excellent acoustic propertiesApplications: Dust Control, Playground, Running Track, Soil Stabilization and Sound DampeningNorth AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 48 %
48 %
pH 8.7
8.7
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 0.000 °C
32.0 °F
Users viewing this material also viewed the following: