Styron DL 2219LA Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 2219LA Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: General purpose, high adhesion to paper and olefin substrates, medium stiffnessApplications: General Purpose AdhesiveLatin America/South AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 45.5 %
45.5 %
pH 9.5
9.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -30.0 °C
-22.0 °F