Styron DL 218NA Carboxylated SB

Category Polymer , Thermoplastic , Styrene-Butadiene
Manufacturer Styron
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DL 218NA Carboxylated SB.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Performance Features: Non-yellowing, high stiffness, anti-sag, mineral binderApplications: Flooring Felt and Leather BindingNorth AmericaInformation provided by Styron
Physical Properties Metric English Comments
Solids Content 47 %
47 %
pH 5.5
5.5
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 97.0 °C
207 °F