Styron DGF080.00 ESU Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Styron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styron DGF080.00 ESU Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Overview: 10% glass filled polypropyleneNaturalMedium flowHeat ResistantInformation provided by Styron
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
ASTM D792
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Yield 21.6 MPa
3130 psi
ISO 527-2
Flexural Modulus 1.40 GPa
203 ksi
ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature -40.0 °C
2.86 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
Unannealed; ISO 75-2/Bf
Deflection Temperature at 1.8 MPa (264 psi) 52.0 °C
126 °F
Unannealed; ISO 75-2/Af
Flame Spread 35.0 mm/min
1.38 in/min
ISO 3795