Styrolution Terlux® 2802 HD MABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer Styrolution
Trade Name Terlux®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terlux® 2802 HD MABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Terlux 2802 HD is a standard injection molding Methyl Methacrulate Acrylonitrile Butadiene Styrene grade for transparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 0.35 %
0.35 %
50% RH; ASTM D570
0.70 %
0.70 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.01397 cm/cm
0.01397 in/in
1/8" bar
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D638
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D638
Glass Transition Temp, Tg 107 °C
225 °F
ASTM D3418
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm

@Thickness 1.50 mm
>= 1.00e+13 ohm-cm

@Thickness 0.0591 in
ASTM D257
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ASTM D257
Descriptive Properties Value Comments
Commercial Status North America
Users viewing this material also viewed the following: