Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Styrolution Terblend® N NM-19 ABS/PA6 (Dry)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer Styrolution
Trade Name Terblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Styrolution Terblend® N NM-19 ABS/PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Terblend N NM-19 is a UV stabilized ABS/PA6 blend combining very high impact strength, even at low temperatures with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 1.4 %
1.4 %
23°C/50% R.H.; ISO 62
Melt Flow 19 g/10 min

@Load 10.0 kg,
Temperature 240 °C
19 g/10 min

@Load 22.0 lb,
Temperature 464 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 36.0 MPa
5220 psi
0.2 in/min; ASTM Test
Tensile Strength, Yield 43.0 MPa
6240 psi
50mm/min; ISO 527
45.0 MPa
6530 psi
2 in/min; ASTM Test
Elongation at Break >= 50 %
>= 50 %
50mm/min, Nominal strain; ISO 527
>= 50 %
>= 50 %
0.2 in/min; ASTM Test
Elongation at Yield 3.5 %
3.5 %
50mm/min; ISO 527
Tensile Modulus 1.93 GPa
280 ksi
ASTM Test
2.00 GPa
290 ksi
1mm/min; ISO 527
Flexural Strength 62.0 MPa
8990 psi
ISO Data
Flexural Modulus 1.80 GPa
261 ksi
ISO Data
Izod Impact, Notched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
ISO Test
Charpy Impact Unnotched NB
NB
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179
Charpy Impact, Notched 7.00 J/cm²
33.3 ft-lb/in²
ISO 179
1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
ISO 179
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °C
195 °F
ASTM Test
95.0 °C
203 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM Test
70.0 °C
158 °F
ISO 75
Vicat Softening Point 103 °C
217 °F
(50 °C/h / 50N) - B/50; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Dielectric Constant 2.9

@Frequency 1.00e+6 Hz
2.9

@Frequency 1.00e+6 Hz
IEC 60250
3.3

@Frequency 100 Hz
3.3

@Frequency 100 Hz
IEC 60250
Dielectric Strength 41.0 kV/mm
1040 kV/in
IEC 60243-1
Dissipation Factor 0.015

@Frequency 1.00e+6 Hz
0.015

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Commercial Status North America and Europe
Primary Processing Technique Injection Molding
UL.UL-C Yes
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved