Material Notes:
Extrusion grade, high gloss.Applications: Extruded sheets requiring medium property levels, profiles, blow molding parts.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Water Absorption 0.30 %
0.30 %
Saturation in water
Water Absorption at Saturation 0.30 %
0.30 %
Melt Flow 7.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
7.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
Elongation at Yield 2.3 %
2.3 %
Tensile Modulus 2.50 GPa
363 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C
201 °F
Vicat Softening Point 101 °C
214 °F
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
Dielectric Strength 34.0 kV/mm
864 kV/in
Dissipation Factor 0.0070

@Frequency 1e+6 Hz
0.0070

@Frequency 1e+6 Hz
0.0090

@Frequency 100 Hz
0.0090

@Frequency 100 Hz
Comparative Tracking Index 600 V
600 V