Struktol V-PEAS VG LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol V-PEAS VG LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
STRUKTOL® V-PEAS VG is a very effective lubricant with externally lubricating properties which has no negative impact on clarity in extrusion, calendaring, or injection molding. STRUKTOL® V-PEAS VG is noted to have ideal characteristics for calendared sheet where clarity is critical and where lower cost in performance is needed to replace montanic esters.Applications: STRUKTOL® V-PEAS VG (Vegetable Grade) is a very compatible complex ester lubricant manufactured from vegetable source fatty acids and is especially suited for calendared PVC sheet. It also has application in extrusion, blow molding and injection molding formulations.Information provided by StruktolSanctioned for use by the Food and Drug Administration in a number of applications, listed in the following sections of Title 21 of the Code of Federal Regulations: 178.3690
Physical Properties Metric English Comments
Specific Gravity 1.028 g/cc
1.028 g/cc
Thermal Properties Metric English Comments
Dropping Point 52.0 - 60.0 °C
126 - 140 °F
Chemical Properties Metric English Comments
Acid Value 5.0 - 12
5.0 - 12
Processing Properties Metric English Comments
Shelf Life >= 24.0 Month
>= 24.0 Month
Descriptive Properties Value Comments
Appearance Off-white powder or pastille