Struktol TPW 101 Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TPW 101 Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mixture of zinc stearate and waxes.STRUKTOL® TPW 101 is a general-purpose blend of lubricants designed to provide improved processing characteristics of highly filled polyolefin compounds. This product will improve filler dispersion and provide metal release for both molding and extrusion operations.
Physical Properties Metric English Comments
Specific Gravity 0.955 g/cc
0.955 g/cc
Additive Loading 2.0 - 6.0 %
2.0 - 6.0 %
Depending on filler loading and process requirements
Thermal Properties Metric English Comments
Dropping Point 110 - 120 °C
230 - 248 °F
Descriptive Properties Value Comments
Appearance Off-white pastilles or beads