Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name STRUKSILON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
STRUKSILON 8120 was developed as universal silicone stabilizer of high potency for the production of conventional as well as flame retardant flexible polyurethane slabstock foam based on polyether polyols.Applications: STRUKSILON 8120 is applicable in systems for nearly all known flexible PU slabstock foam applications and technologies like production of seats, chairs, mattresses etc. in the furniture and automotive industry and for all kinds of damping devices.Information provided by Struktol
Physical Properties Metric English Comments
Density 1.023 g/cc
0.03696 lb/in³
Viscosity 900 cP

@Temperature 25.0 °C
900 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Optical Properties Metric English Comments
Refractive Index 1.449

@Temperature 25.0 °C
1.449

@Temperature 77.0 °F
Descriptive Properties Value Comments
Appearance Clear, colorless to slightly yellow liquid
Turbidity Point °C 34