Struktol STRUKSILON 8007 Silicone Stabilizer for PU-Rigid Foam

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name STRUKSILON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol STRUKSILON 8007 Silicone Stabilizer for PU-Rigid Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
STRUKSILON 8007 was developed as universal silicone stabilizer for production of polyurethane rigid foam based on polyester and polyether polyols.Applications: STRUKSILON 8007 is applicable in combination with the usual blowing agents in systems for nearly all known PU rigid foam applications, e.g. sandwich elements (CLBS), insulation material for production of cooling and heating appliances and facilities, roof and wall insulations in the construction industry and for systems in the block foam area.Information provided by Struktol
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Viscosity 900 cP

@Temperature 25.0 °C
900 cP

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
DIN/ISO 2562
Optical Properties Metric English Comments
Refractive Index 1.4515
1.4515
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in closed original containers if transported and stored at temperatures between 1 and 30°C
Descriptive Properties Value Comments
Appearance Clear, colorless to slightly yellow liquid
Turbidity Point °C 31