Struktol POLYDIS 3615 Elastomer modified epoxy prepolymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Epoxy
Manufacturer Struktol
Trade Name POLYDIS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol POLYDIS 3615 Elastomer modified epoxy prepolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: STRUKTOL VP 3615 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural and peel strength. Contrary to PD 3614 the Tg decrease less, but fracture toughness is on the same level.Information provided by Struktol
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Viscosity 250000 cP

@Temperature 25.0 °C
250000 cP

@Temperature 77.0 °F
Dynamic
Chemical Properties Metric English Comments
Acid Value <= 1.0
<= 1.0
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in original sealed containers at temperatures less than 40°C
Descriptive Properties Value Comments
Appearance Yellowish, high viscous epoxy resin
Elastomer Content % 40 NBR
Epoxy Equivalent Weight (g/Eq) 300
Resin-base of the prepolymer DGEBA