Struktol POLYDIS 3614 Elastomer modified epoxy prepolymer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoset , Epoxy
Manufacturer Struktol
Trade Name POLYDIS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol POLYDIS 3614 Elastomer modified epoxy prepolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: STRUKTOL POLYDIS 3614 is used where conventional epoxy systems are unable to satisfy the demands of for example impact, flexural or peel strength. This prepolymer type causes best low temperature flexibilisation and adhesion on oily steel.Information provided by Struktol
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Viscosity 470000 cP

@Temperature 25.0 °C
470000 cP

@Temperature 77.0 °F
Dynamic
Chemical Properties Metric English Comments
Acid Value <= 1.0
<= 1.0
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month
>= 12.0 Month
in original sealed containers at temperatures less than 40°C
Descriptive Properties Value Comments
Appearance Yellowish, high viscous epoxy resin
Elastomer Content % 40 NBR
Epoxy Equivalent Weight (g/Eq) 330
Resin-base of the prepolymer standard DGEBA