Material Notes:
PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (Fused Deposition Modeling) systems manufacture parts using PPSF/PPSU material that are not only mechanically superior, but also dimensionally accurate, accurately predicting end-product performance. Users can also sterilize PPSF via steam autoclave, EtO sterilization, plasma sterilization, chemical sterilization and radiation4. PPSF/PPSU gives you the ability to manufacture Real Parts™ direct from digital files.Information provided by Stratasys®
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 86
86
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
Type 1, 2"/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 2.068 GPa
299.9 ksi
Type 1, 2"/min; ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.206 GPa
320.0 ksi
ASTM D790
Izod Impact, Notched 0.5873 J/cm
1.100 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.655 J/cm
3.100 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 189 °C
372 °F
ASTM D648
Glass Transition Temp, Tg 230 °C
446 °F
DMA (SSYS)
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Constant 3.45

@Frequency 60.0 Hz
3.45

@Frequency 60.0 Hz
IEC 60250
Dielectric Strength 14.6 kV/mm
371 kV/in
IEC 60112