Stir SpA Z 74 AT 1 (PVC)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Stir SpA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stir SpA Z 74 AT 1 (PVC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: Molding for beach footwearInformation provided by STIR SpA
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ISO 1183
Density 0.680 g/cc
0.0246 lb/in³
Foamed Density; ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
ISO 868
Tensile Strength at Break 15.9 MPa
2310 psi
ISO R 527
Elongation at Break 351 %
351 %
ISO R 527
Abrasion 141
141
Close, mm³; ISO 4649
272
272
Foam, mm³; ISO 4649